Table 1 Affinities of CBM-variants for birch wood xylanas determined by affinity electrophoresis

From: Synthetic xylan-binding modules for mapping of pulp fibres and wood sections

Protein KD (mg/ml) Relative affinity (%)
wt CBM4-2 0.12 100
X-2 0.22 52
X-6 0.07 157
X-13 1.00 12