Table 1 The number-average molecular weight (MN), weight-average molecular weight (MW) and rubber particle size of latex from 1-year virgin trees and 30-year-old regularly tapped trees of Reyan7-33–97 and RRIM600 clones

From: Comparative analysis of latex transcriptomes reveals the potential mechanisms underlying rubber molecular weight variations between the Hevea brasiliensis clones RRIM600 and Reyan7-33–97

Latex Samples MN (× 104) MW (× 105) MWD (MW/MN) Geometric Mean Diameter (μm)
Reyan73397y1 8.62 ± 1.84 4.77 ± 0.65 5.53 0.72
RRIM600y1 7.18 ± 0.39 4.26 ± 0.22 5.94 0.69
Reyan73397y30 9.05 ± 2.16 6.51 ± 0.88 7.19 0.85
RRIM600y30 17.73 ± 4.78 8.28 ± 0.58 4.67 0.79